HAADGEMISK ELEMENTEN EN EIGENSKAPPEN
Eigenskippen \ Graad | | | | | | A1 | |
| | Cr | Al | | Re | Fe |
| | | | | 25.0 | 6.0 | | Geskikt | Lykwicht |
Maks. trochgeande tsjinsttemperatuer (ºC) | | Diameter 1.0-3.0 | | Diameter grutter as 3.0, |
| 1225-1350℃ | | | 1400℃ |
| | | | | | | |
Wjerstân 20ºC (ohm*mm²/m) | | | | 1.45 | |
| Dichtheid (g/cm3) | | | | | 7.1 | |
Ungefear smeltpunt (ºC) | | | | 1500 | |
| Ferlinging (%) | | | | | 16-33 | |
Werhelle bûgfrekwinsje (F/R) 20℃ | | | | 7-12 | |
Kontinue tsjinsttiid 1350℃ | | | Mear as80 oeren |
| | | | | | | |
Mikrografyske struktuer | | | | Ferriet | |
|
Oven | | Droege loft | | Fochtige loft | | wetterstof-argon | Argon | Untbining |
atmosfear | | | | | | gas | | | | ammoniakgas |
Temperatuer(℃) | | 1400 | | 1200 | | 1400 | | 950 | 1200 |
Brûkershânlieding
- Nominale spanning: 220V/380V
- Om te foarkommen dat de kachel fochtich wurdt, moatte se by it ynstallearjen wanten drage. De tried moat ynstalleare wurde nei't de kachel flak bleaun is, om krassen op it oerflak, smoargens, korrosje of ferkearde ynstallaasje te foarkommen, wat ynfloed hat op 'e libbensdoer fan 'e kachel.
- Yn 'e nominale spanning om te brûken. Yn sterke redusearjende sfearen, soere sfearen, in sfear fan hege fochtigens sil ynfloed hawwe op it gebrûk fan 'e libbensduur;
- De temperatuer foar gebrûk moat yn in droege, net-korrosive atmosfear wêze, en moat in pear oeren by in temperatuer fan sawat 1000 ℃ wêze, sadat nei normaal gebrûk in beskermjende film op it oerflak ûntstiet, om de normale libbensdoer fan 'e oventried te garandearjen;
- By it ynstallearjen fan 'e oven moat derfoar soargje dat de isolearre tried goed stroom leveret, sadat de tried net oanrekke wurdt troch de oven nei de tried, en dat der gjin elektryske skokken of brânwûnen foarkomme.
Foarige: Kan-thal APM Fecral Alloys Hege temperatuer hjittebestindige elektryske tried Folgjende: FeCrAl A1 APM AF D-legering hjittebestindige elektryske tried