1.GemyskCkomposysje
Materiaal | Gemyske gearstalling (%) | ||||
Ni | Cr | Si | Mn | Al | |
KP (Chromel) | 90 | 10 | |||
KN (Aluminium) | 95 | 1-2 | 0.5-1.5 | 1-1.5 |
2.Fysyske eigenskippenen Mechanyske eigenskippen
Materiaal | Dichtheid (g/cm3) | Smeltpunt ℃) | Treksterkte (Mpa) | Folume-resistinsje (μΩ.cm) | Ferlingingssnelheid (%) |
KP (Chromel) | 8.5 | 1427 | >490 | 70.6 (20℃) | >10 |
KN (Aluminium) | 8.6 | 1399 | >390 | 29.4 (20 ℃) | >15 |
3.EMF-weardeberik by ferskillende temperatueren
Materiaal | EMF-wearde tsjin Pt(μV) | |||||
100 ℃ | 200 ℃ | 300 ℃ | 400 ℃ | 500 ℃ | 600 ℃ | |
KP (Chromel) | 2816~2896 | 5938~6018 | 9298~9378 | 12729~12821 | 16156~16266 | 19532~19676 |
KN (Aluminium) | 1218~1262 | 2140~2180 | 2849~2893 | 3600~3644 | 4403~4463 | 5271~5331 |
EMF-wearde tsjin Pt(μV) | ||||
700 ℃ | 800 ℃ | 900 ℃ | 1000 ℃ | 1100 ℃ |
22845~22999 | 26064~26246 | 29223~29411 | 32313~32525 | 35336~35548 |
6167~6247 | 7080~7160 | 7959~8059 | 8807~8907 | 9617~9737 |
TYPE K (CHROMEL tsjin ALUMEL)wurdt brûkt yn oksidearjende, inerte of droege redusearjende atmosfearen. Bleatstelling oan fakuüm beheind ta koarte perioaden. Moat beskerme wurde tsjin swevelrike en marzjinaal oksidearjende atmosfearen. Betrouber en krekt by hege temperatueren.